Modern Manufacturing Engineering ›› 2024, Vol. 522 ›› Issue (3): 156-160.doi: 10.16731/j.cnki.1671-3133.2024.03.021

Previous Articles    

Experimental study on friction characteristics of cryogenic rolling bearing materials

REN Jiongli1, SU Bing1, LIU Fengbo1, ZHANG Guangtao1, LIU Peng2, ZHANG Wenhu1   

  1. 1 School of Mechanical Engineering,Henan University of Science and Technology,Luoyang 471003,China;
    2 Luoyang Bearing Research Institute Co.,Ltd.,Luoyang 471003,China
  • Received:2023-05-04 Online:2024-03-18 Published:2024-05-31

Abstract: The friction characteristics of silver (Ag),polytetrafluoroethylene (PTFE) and molybdenum disulphide (MoS2) coatings were tested under different contact stresses and different sliding speeds using a high-speed rotary friction and wear tester in an ultra-low temperature liquid nitrogen (LN2) environment.The shape of the wear marks and the main components of the steel discs were analysed using an XM-200 surface morphometer,a JSM-7800F scanning electron microscope (SEM) and an energy spectrometer (EDS),and the friction factors and wear mechanisms of the three coatings were investigated under ultra-low temperature environment. The results show that the friction factor of the coated steel discs does not vary much under two speeds (high sliding speed of 2 m/s and low sliding speed of 0.4 m/s),while the friction factor of the uncoated steel discs is influenced by the sliding speed,with MoS2 and PTFE having the best friction reduction effect.The wear of the three coatings increases with increasing load for the same operating conditions.The wear resistance of PTFE in the ultra-low temperature environment is poor and the wear amount is higher,while the wear amount of steel/MoS2 coating is the smallest and steel/Ag coating is the second,indicating that both Ag and MoS2 show good wear resistance in the ultra-low temperature environment and the wear amount is smaller.

Key words: cryogenic environments, solid lubrication, coating materials, frictional wear